Publicación: Performance study of slurry aluminide coated 347H immersed in Li-Na-K carbonate molten salt for 5000-h at 700 °C
Fecha
2025-10-06
Título de la revista
ISSN de la revista
Título del volumen
Editor
Elsevier
Resumen
Concentrated Solar Power (CSP) systems coupled with thermal energy storage (TES) are increasingly considered to provide dispatchable, low-carbon energy. To further improve their performance, next-generation CSP plants are designed to operate under more severe conditions, which raises concerns regarding high-temperature corrosion of structural materials by molten salts. This study examines the corrosion behaviour of bare and slurry aluminide-coated 347H stainless steel after exposure to a Li–Na–K carbonate eutectic at 700 °C for up to 5000 h. The uncoated alloy showed rapid degradation, characterized by a brittle, multi-layered oxide scale, extensive internal oxidation, and carburization. The outer oxide layer consisted mainly of LiFeO₂ and LiMnO₂, while the internal oxidation zone contained (Fe,Cr)₃O₄ spinels, LiCrO₂, and Ni-rich metallic islands. In contrast, the aluminide-coated samples exhibited excellent corrosion resistance without spallation or mechanical failure. The coating transformed into a compact FeAl layer, overlaid by a dense oxide composed of α- and γ-LiAlO₂. The α-LiAlO₂ phase, forming at the oxide–coating interface via the reaction of Al₂O₃ with lithium oxide, acted as a continuous and chemically stable barrier. Its persistence during exposure was key to prevent molten salt ingress and ensure long-term protection. These findings demonstrate that slurry aluminide coatings effectively increase the durability of structural alloys in molten carbonate environments relevant for advanced CSP-TES applications.
Descripción
Highlights
Molten carbonate corrosion of coated and uncoated 347H was investigated at 700 °C.
Bare 347H forms multi-scale Li-rich and spinel oxides and undergoes carburization.
Newly developed slurry aluminide coating provides corrosion resistance over 5000 h.
Coating slowly transforms into compact FeAl layer due to continuous Al-diffusion.
Continuous α-LiAlO2 layer forms at coating surface, ensuring long-term protection.
Palabras clave
Slurry aluminide
Citación
Surface and Coatings Technology 517: 132762